Digitální knihovna UPCE přechází na novou verzi. Omluvte prosím případné komplikace. / The UPCE Digital Library is migrating to a new version. We apologize for any inconvenience.

Publikace:
Protection of hematite photoelectrodes by ALD-TiO2 capping

Článekopen accesspeer-reviewedsubmitted version (preprint)
Načítá se...
Náhled

Datum

Autoři

Imrich, T
Zazpe, Raul
Krysova, H
Pausova, S
Dvořák, Filip
Rodriguez Pereira, Jhonatan
Michalicka, J
Man, O
Macák, Jan
Neumann-Spallart, M

Název časopisu

ISSN časopisu

Název svazku

Nakladatel

Elsevier Science SA

Výzkumné projekty

Organizační jednotky

Číslo časopisu

Abstrakt

Iron (III) oxide, in the form of hematite (alpha-Fe2O3), is a n-type semiconductor which is photoactive in the visible spectral region. Therefore, use in photoelectrocatalysis and photoassisted water electrolysis may be suggested. For such implementations, stability of contacts with liquid phases is mandatory. Hematite is stable in alkaline media but less stable in acidic media. For the first time the coverage of porous photoactive Sn doped hematite by thin capping layers of TiO2, deposited by Atomic Layer Deposition (ALD) and its impact on photocurrent and chemical stability of hematite is shown. The nominal thicknesses of the TiO2 ALD coatings were 0.5, 2 and 7.5 nm. The presence of the TiO2 coatings was evidenced by X-ray photoelectron spectroscopy, high-resolution transmission electron microscopy (HR-TEM) and scanning TEM coupled with energy dispersive X-ray (EDX) spectroscopy. HR-TEM analyses revealed that the TiO2 capping layers were amorphous and conformal. Exposure of uncovered hematite layers to 1 M sulfuric acid led to a nominal dissolution rate of 0.23 nm/h which was halved when a TiO2 ALD coating (7.5 nm thin) was applied. Due to mismatch of the valence band positions of the two semiconductors, photocurrents were strongly diminished as the capping layer thickness was increased. Post calcination of as deposited ALD films on hematite resulted in an increase of photocurrent, which only exceeded photocurrents of pristine hematite when the ALD thickness was not more than 0.5 nm.

Popis

Klíčová slova

hematite, TiO2 capping layer, chemical dissolution, ALD, XPS, hematit, ochranná TiO2 vrstva, chemické rozpouštění, ALD, XPS